ACADEMY SERIES · EPISODE 35Paint Shops
Is the Air Behind Your Paint Defects?
If you see orange peel, craters or adhesion problems, the source may be the air. We cover flash rust, the effect of too much and too little humidity on paint, and how the balance is achieved.
Published: 9 November 2026Narration: Turkish and English2:27
In this video
- Blasted steel is highly reactive; flash rust can form within minutes in humid conditions.
- This rust reduces adhesion and often means blasting again.
- Too much humidity slows solvent evaporation, can haze epoxy and polyurethane and lengthens water based drying.
- In dry air static attracts dust, and orange peel, craters and marks can increase.
- The aim is balance: dry air in humid periods, humidification in dry periods.
More from this series
Academy Series · Ep. 1
Moisture Load Calculation
Psychrometrics & Sizing · 4 October 2026
Academy Series · Ep. 2
Relative Humidity and Health
Health & Indoor Climate · 3 October 2026
Academy Series · Ep. 3
Dehumidification Technologies
Technology Selection · 4 October 2026
Academy Series · Ep. 4
Dehumidifier Selection
Equipment Selection · 4 October 2026
Academy Series · Ep. 5
How to Calculate Humidification Load
Humidification Load · 5 October 2026
Academy Series · Ep. 6
Humidity Control in Swimming Pools
Pool Humidity Control · 5 October 2026